Other Materials Fatigue File Directory :
Updates: Jan2012, Jul2025
Note! : The pages and files in this directory are offered by the
F.D.+ E. committee members as a set of example files for the
construction of web based material fatigue property databases.
They are meant for information and research use only, not for design.
Copper Based
- Copper, Annealed (Hatanaka 1990)
- OHFC Copper, Annealed (Nachtigall, NASA 1974)
- OHFC Copper, Annealed, -195C (Nachtigall, NASA 1974)
- OHFC Copper, Annealed, -269C (Nachtigall, NASA 1974)
- W.D.France, D.E.Trout, J.A.Mulholland 1969
Warning!! : Cantelever bending data, Assumed NO plasticity!
- Bronze 210, hard
- CartridgeBrass 260, hard
- CartridgeBrass 260, Spring
- Bronze 405, hard
- Bronze 408, hard
- SpringBronze 430, hard
- SpringBronze 430, hard
- SpringBronze 430, hard
- SpringBronze 430, Spring
- SpringBronze 434, hard
- SpringBronze 434, Spring
- PhosphorBronze 510, hard
- PhosphorBronze 510, Spring
- PhosphorBronze 521, hard
- PhosphorBronze 521, Spring
Nickel Based
- Inconel IN718 Room Temp. (Nachtigall 1974)
__ | __ Fitted
__ | __ Calculator
- Brinkman/Korth 1976 Inconel IN718
( Note: no direct correlation between Strain-Stress-Life and
Elas.mods not reported, made it difficult to create these files.
Check with the original paper. )
- Tensile Curves, Engr. Stress-Strain
- HeatTreat at 1038C, Test at 22C
__ | __Fitted
__ | __Calculator
- HeatTreat at 1038C, Test at 427C
__ | __Fitted
__ | __Calculator
- HeatTreat at 1038C, Test at 538C
__ | __Fitted
__ | __Calculator
- HeatTreat at 1038C, Test at 650C
__ | __Fitted
__ | __Calculator
HT 1038C, all Strain-Life plots
HT 1038C, all stress plots
HT 1038C, all Neuber stress plots
- HeatTreat at 940C, Test at 22C
__ | __Fitted
__ | __Calculator
- HeatTreat at 940C, Test at 538C
__ | __Fitted
__ | __Calculator
- HeatTreat at 940C, Test at 650C
__ | __Fitted
__ | __Calculator
HT 1038C, all Strain-Life plots
HT 1038C, all stress plots
- Inconel IN718 Temp.= 650C
HeatTreat2, heat 1 (Brinkman/Korth 1976)
- Inconel IN718 Temp.= 650C
HeatTreat2, heat 2 (Brinkman/Korth 1976)
- Inconel IN718 Temp.= 650C
HeatTreat2, heat 3 (Brinkman/Korth 1976)
- Inconel IN718 Temp.= 650C
HeatTreat2, all 3 above merged (Brinkman/Korth 1976)
__ | __ Fitted
__ | __ Calculator
- Inconel IN738LC Room Temp. (Guo/Ranucci 1983)
(Not enough data for a fitted curve or calculator.)
- Inconel X Room Temp. (Smith et al NASA)
- Inconel 625 Tested at 540C. (G.D.Smith et.al. 1996)
Beryllium
Back to Materials Index