# keyhManTenTens.txt # ManTen Steel USS Co, SAE1320 Weathering Steel # Chem. .23Cwt% 1.57Mn .016P .022S .01Si .22Cu # 3/8 inch thick plate, hot rolled. # Ref.: L.Tucker, S.Bussa, "The SAE Cumulative Fatigue Damage Test # Program," SAE paper 750038, SAE Congress Detroit MI, Feb. 1975. # Long life data has been adjusted arbitrarily to 50% of CA Fat.Limit # NOTE!: For BS7910 FADs required Tags are: # #FileType= #DataType= #Sy= #Su= #E= # #Stress_units= #Strain_units= # #FileType= strain_stress #DataType= engineering #Can be "engineering" or "true" #Name= ManTenFDE #Name= SAE1320+Cu #Name= CopperSteel #Stress_units= mpa #Strain_units= strain #Sy= 322 mpa avg. of 3 #Su= 556 #E= 206000 mpa 29900 ksi reported #BHN= 169 based on Su #%RA= 67 % #TrueFractureStress= 990 mpa #TrueFractureStrain= 1.06 #monotonicK= 997 mpa #monotonicn= 0.21 #Strain Stress 0. 0. 0.0005293 106.41 0.0009249 185.58 0.0015664 318.86 0.0017481 355.18 0.0018871 378.42 0.0019997 362.42 0.0022193 342.41 0.0024174 323.85 0.0028189 323.81 0.0040394 326.58 0.0056345 330.76 0.0068496 334.98 0.0079951 338.85 0.0103611 350.57 0.0115815 356.97 0.0127752 365.56 0.0143488 378.1 0.0159011 391